中田 克弥, 森賀 俊広 : Synthesis and sintering behavior of La0.3Sr0.7TiO3 powders for SOFC interconnector using spray pyrolysis method, Outstanding Presentation, 2nd International Forum on Advanced Functional Materials and Polymer Materials @ Qingdao R&D Institute, Xi'an Jiaotong University, 2016年10月.
欧文冊子 ●
NAKATA KatsuyaandToshihiro Moriga : Synthesis and sintering behavior of La0.3Sr0.7TiO3 powders for SOFC interconnector using spray pyrolysis method, Outstanding Presentation, 2nd International Forum on Advanced Functional Materials and Polymer Materials @ Qingdao R&D Institute, Xi'an Jiaotong University, Oct. 2016.